| > the nails are only there to hold it until the glue dries This is a phrase my brother, a cabinet maker/ jointer, uses... And tests occasionally: Glue 2 pieces of timber together at 90 degrees and clamp it normally. When dry, break the join (by bashing it with a hammer is his general way) to see if it's the glue or the timber. Nearly all of the glue he tests are stronger than the timber (Oz, US and Asian hardwoods), as it's the timber that is ripped apart, and not the glue join. A bottle of standard PVA-B (/ exterior grade) from the local hardware store is pretty excellent. When you think about glue, it's everywhere these days. All timber laminates (eg kitchen bench tops, plywood, particle board, MDF, and finger jointed/laminated timber) are just 'glued'. A lot of this is structural timber (ie designed to last decades). From the article: > This joint failed by the wood in the post shearing along the growth rings This is the most common place of failure when witnessing my brother's "tests", and makes a lot of sense it happens that way too. The glue should have been the strongest part of ALL of his tests. It looks like he 'over clamped' the timber (ie squeezed out all the glue) in few of his photos [0]: which is something my brother has warned me about, as it makes the join weak. [0] https://woodgears.ca/joint_strength/failures.html Edit: clarification |